This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2020, 11, 899–910, doi:10.3762/bjnano.11.75
Figure 1: a) SEM images of ZnMgO films deposited on p-Si substrates by spin coating (left column) and aerosol...
Figure 2: a) SEM image of a ZnMgO film prepared by aerosol spray pyrolysis. b) SEM image of a ZnMgO film prep...
Figure 3: Elemental composition of a ZnO (a) and a Zn0.6Mg0.4O (b) film determined by EDAX analysis.
Figure 4: PL spectra of Zn1−xMgxO films deposited by spin coating with x values of 0.00 (1); 0.05 (2); 0.15 (...
Figure 5: PL spectra of Zn1−xMgxO films deposited by spin coating with x values of 0.00 (1); 0.10 (2); and 0....
Figure 6: a) XRD pattern of a Zn0.8Mg0.2O film deposited by spin coating on a Si substrate and annealed at 50...
Figure 7: A model for the band tails distribution at 20 K in Zn1−xMgxO films with the x value composition of ...
Figure 8: PL spectra of Zn0.85Mg0.15O films by spin coating (curve 1) and aerosol spray pyrolysis (curve 2) m...
Figure 9: Current–voltage characteristics in dark and under UV illumination for a p-Si/n-Zn0.9Mg0.1O heterost...
Figure 10: Current–voltage characteristics in dark and under UV illumination for a p-Si/n-Zn0.6Mg0.4O heterost...